Quality Aluminum Casting parts of distributing pipe ADC12 for Sale

Min. Order: 4000 Piece/Pieces
inquiry

Basic Info

——

Model No.: L017100

Material: Aluminum

Deck: Double

Muffler Type: Rear Muffler

Type: Windscreen Wiper System

Surface Finish: Electrophoresis Coating

Weight: 200g-3000g

Cavity Number: 2

Additional Info

——

Packaging: carton, PE pallet, PE flow box, steel box, wooden pallet, container

Productivity: 20000/MONTH

Brand: NONE

Transportation: Ocean,Land,Air

Place of Origin: NINGBO

Supply Ability: 200000/MONTH

Certificate: IATF16949:2016,ISO14001:2015,ISO45001:2018

HS Code: 7616991090

Port: NINGBO,SHANGHAI

Product Description

——

Aluminum Casting parts of distributing pipe ADC12, 


the material for this part is ADC-12, a kind of material, having good fluidity, which is good for filling while die casting. This material is a good material to produce end cover, housing, gearbox, bracket etc. The composition of ADC-12 is:(Cu)1.5~3.5, (Si)9.6~12.0, (Mg)≤0.3, (Zn)≤1.0, (Fe)≤1.3, (Mn)≤0.5, (Ni)≤0.5, (Sn)≤0.3, (Pb) ≤0.1, (Cd) ≤0.005, (Al) the remaining.


The cavity number for this part is 1 , according to the required tolerance and dimensions in terms of the prints, the part has difficulty on CNC machining, the wall thickness is small, not much machining allowance left. The part is a kind of distributing pipe.


For this product, we should pay close attention to deformation

Features: the overall deformation of the casting geometry does not meet the design requirements.
Causes
1, the casting structure design is bad, cause uneven contraction.
2, mold opening too early, casting rigidity is not enough.
3, too small casting inclination.
4. Improper operation of casting.
5. Improper placement of push rod.


Exclusion measures


1, improve the casting structure, so that the wall thickness uniformity.
2, determine the best mold opening time, strengthen the casting rigidity.
3. Enlarge the inclination of casting.
4, take the casting should be careful, handle with care.
5. The application of special box for casting and the way of removing gate should be proper.
6. Some deformed castings can be eliminated by shaping.

Material: ADC-12

Cavity Number: 1
Process Technology: High pressure die casting, Cold Chamber
Product Dimensions: Customized
Casting General Tolerance: Grade GB-CT4
Surface Finish: Polishing, Shot Peening
Flow Processes: Die casting, Degating, Deburring to remove the flash around the ejector pins, Polishing to remove the parting line, Shot peening to make the part more consistency,CNC Milling, Cleaning, Packaging, Shipping
Control Measure: Incoming Material Test, First Article inspection, Routing inspection, Final item inspection,  and Outgoing quality control
Inspection Equipment: CMM, Caliper, Plug Gage, Screw Gauge
Application: Auto Parts
Certificate: IATF16949:2016,ISO14001:2015,ISO45001:2018
Lead Time: 30-35 days
Trade Term: FOB Ningbo

024 Aluminum Casting Parts Of Distributing Pipe Adc12 2022 05 23 01 Jpg

BOLANG PLANTDIE CASTING MACHINE

CNC work shop


CMM facility

Products