Min. Order: | 4000 Piece/Pieces |
---|
Model No.: L027806
Material: Aluminum
Deck: Double
Muffler Type: Rear Muffler
Type: Muffler Assembly
Weight: 200g-3000g
Cavity Number: 1
Surface Finish: Polishing
Machine: Cold Chamber
Packaging: carton, PE pallet, PE flow box, steel box, wooden pallet, container
Productivity: 5000/MONTH
Brand: NONE
Transportation: Ocean,Land,Air
Place of Origin: NINGBO
Supply Ability: 6000/MONTH
Certificate: IATF16949:2016,ISO14001:2015,ISO45001:2018
HS Code: 7616991090
Port: NINGBO,SHANGHAI
Aluminum die casting parts of Material position device case&cover ADC12, the parts are used in the conveyer equipment on the motor facility, the part have 2 cavities, so on the mold, there will be many protrude from the surface, then while feeding the mold, as the injection gate is located at the bottom of the surface, so when the high-speed molten aluminum is injected, it will hit the big protruded feature, leading to eddy or turbulence, what's more, because of the big round feature, sometimes the molten aluminum will start to be solid at the back area of the feature though not fill sufficiently, leading to cold shut, or shrinkage porosity. Meanwhile, the top of the part will also be a position with high risk of feeding problem, as it is far-distance end on the part, the most difficult area for aluminum to reach. For such problem, the control method is to increase the temperature of the molten aluminum, to supervise the die temperature with infrared thermometer.
Then, during actual production, the operator should work under the process parameters set up by the engineering according to the operation instruction. Visual inspect the condition of the castings at the back surface, no defect such as cold shut is allowed. The inspector also should attach importance to the color difference from the back area and front area. For the top area of the part, the two bosses are required to be tapped, so the CNC workshop should take a couple of pcs to have trial machining to observe is there is porosity at this area. If the filling of the casting is not well, the bosses may happen to be broken, or with careful visual inspection, we may find color difference at the boss, which like weld mark, how it comes? It is when two aluminum flow with different temperature come across but not merge well. In this case, the part will be easily broken at this joint surface, resulting in the scrap of the part.
Material: ADC12
Cavity Number: 2
Process Technology: High pressure die casting, Cold Chamber
Product Dimensions: Customized
Casting General Tolerance: Grade GB-CT4
Surface Finish: Polishing
Flow Processes: Die casting, Degating to remove the residual of the gate, Polishing and Deburring to remove the burrs, Polishing to remove the parting line, flash, High Precision CNC milling Machining, Spray Coating,Assembling,Packaging, Storaging, Shipping
Control Measure: Incoming Material Test, First Article inspection, Routing inspection, Final item inspection, and Outgoing quality control
Inspection Equipment: CMM, Caliper, Plug Gage, Screw Gauge
Application: Motor Parts
Certificate: IATF16949:2016,ISO14001:2015,ISO45001:2018
Lead Time: 30-35 days
Trade Term: FOB Ningbo